Yeah, I thought when I read the sand idea that Fade had a gr8 idea, but as you say, any mistake and you got a mess. I’d much rather use water than sand, as anything dropped into it has a better chance of being salvaged.
I have to believe the fact my source mat is 3 yrs old is having an effect, as yours comes together at such a much lower temp. You’ve taught me patience Guzias, and Fade hasn’t chimed in on any breakdown stuff to suggest it’s a factor (I’m sure it is, but not sure how.)
BTW, my yield on 90g of source mat has been a consistent 5g (twice), which is a very low ratio. I’m thinking that is the biggest result of using 3 yr-old stuff. I have some source mat that was harvested in early Nov., so only 3 months old, am going to be blasting that next. I’m certainly going to be interested to see if I notice reactions sooner.
FWIW, after I verified my stuff returned to shatter, I heated it up a little bit and folded it. I love that part of this, the folding is like pulling taffy. Anyway, fold, fold, fold and it still ended up getting totally clear. There is, IMO, something chemical in the waxing process, not strictly heat/vaq. I’ve no explanation other than it seems to me that you’re achieving wax far easier than I, and I believe you’re source mat is way better than mine…ergo, good source material will wax way easier.
BTW, how does one break up shatter to consume it?
Oh, and I am getting the same bubbling at 136F...so leaving it there.